Process school | common welding defect - wrong mouth
1,the phenomenon of Performance for weld on both sides of the outer wall material is not in the same plane, hi-lo is greater than the amount of 3%~5% or more than 1㎜parentmetalthickness.2.Causeanalysi
2017-09-20 15:56:00.000
Enterprises will be heard to break ground on the digital workshop of | green leaf boiler
Eight in the morning of September15,28points, green leafy boiler was broke ground digital workshop, huang town party secretary qing-fengli,huangtownmayorShaoXiang,greenboilerTanZhidongchairmanChenjian
2017-09-15 15:57:00.000
Welding defects of | common in process school - welding internal slag
1,the phenomenon of The welding process is mixed with impurities such as traditional Chinese medicines kinandotherimpuritiesinthemoltenpool.2.CauseanalysisThecleaningoftheweldingpartsisnotclean,thecoa
2017-09-13 15:57:00.000
"Teacher's day" | lights up the arc
Some people say that the teacheris the brightest north star in the sky, which points out the way forward forus. Somepeoplesaythattheteacherislikethesuns
2017-09-09 15:57:00.000
On 28August afternoon, deputy secretary of municipal party committee of danyang zhi-qiang zhao, huang town partysecretaryqing-fenglilinetoourinvestigation,research,secretaryzhaoalineaccompaniedbytheen
2017-02-10 13:13:00.000
Contact Us
Tel: +86(0)511 86637666
E-mail: marketing@jslygl.com
Address:Zhenjiang Distrit , Jiangsu Province
Pay attention to our
欢迎关注微信公众号
Copyright © 2025 Jiangsu Green Leaf Boiler Co., Ltd. www.300.cn | Tags